> They are pressure treated in a liquid filled tank aka dipped

Immersing a tie in a tank and then pressurizing the tank is "pressure treatment". The pressure treating involves drawing a vacuum first, followed by the application of pressure. This drives the preservative into the tie quite a ways, while plain-old "dipping" merely treats the surface of the wood (and is not very durable).



Subject Written By Date/Time (PST)
  Wooden Ties ? 03-11-2021 - 22:53
  Re: Wooden Ties Rasputin 03-12-2021 - 00:29
  Re: Wooden Ties WebDigger 03-12-2021 - 04:54
  Re: Wooden Ties trackwalker 03-12-2021 - 06:39
  Re: Wooden Ties Greg Hall 03-12-2021 - 09:05
  Re: Wooden Ties An Observer 03-12-2021 - 11:30
  Re: Wooden Ties Dr Zarkoff 03-12-2021 - 11:55
  Re: Wooden Ties An Observer 03-12-2021 - 14:00
  Re: Wooden Ties Rasputin 03-12-2021 - 14:52
  Re: Wooden Ties Dr Zarkoff 03-12-2021 - 15:20


Go to: Message ListSearch
Subject: 
Your Name: 
Spam prevention:
Please, enter the code that you see below in the input field. This is for blocking bots that try to post this form automatically.
 ********  **     **   ******   **     **  ******** 
 **        **     **  **    **  ***   ***     **    
 **        **     **  **        **** ****     **    
 ******    **     **  **        ** *** **     **    
 **        **     **  **        **     **     **    
 **        **     **  **    **  **     **     **    
 **         *******    ******   **     **     **    
This message board is maintained by:Altamont Press
You can send us an email at altamontpress1@gmail.com